Besides the same eutectic with AZS 33 Tile, FUSED CAST AZS 36 Tile has further strengthened anti-erosion ability and reduces the pollution of glass melt because more chain-shape zirconium oxide crystal and low glass phase content. It is suitable for the area with fast glass melt flow rate and high temperature, such as pool wall tiles of the melting tank, pavement tiles and charging mouth tiles.

OSYMEN BRAND

AZS36# ER1685

Al2O3 %

Balance

ZrO2 %

35-40

SiO2 %

≤13.00

Na2O %

≤1.40

Fe2O3+TiO2+CaO+Na2O %

≤2.5

True Specific Gravity, g/cm3

≥3.93

Bulk Density, g/cm3    PT (RN RC N)

ZWS (RR EVF EC ENC)
WS (RT VF EPIC FVP DCL) 

≥3.50

≥3.70

≥3.80

Apparent Porosity, %

≤1.0

Cold crushing strength, Mpa

≥350

Exudation Temperature of Glass Phase, °C

≥1400

Refractoriness under Load T2 , °C

≥1700

Bubble Separation Ratio(1300°C×10h), %

≤1.4

Anti-corrosion rate of glass liquid

1500°C×36h (mm/24h), %

≤1.4